Why is a low-temperature impact test performed on casters? Rotating smoothly in the cold does not mean they won’t crack.

Time:Nov 19,2026

The same caster performs normally at room temperature, but once placed in a cold storage environment, issues such as cracking of the wheel tread or chipping of the rim may occur. What exactly causes this?

In applications such as cold-chain logistics, frozen-food processing, and low-temperature warehousing, casters must not only support the weight of the equipment but also withstand movement and impact in cryogenic environments.

Many procurement professionals focus on a product’s operating temperature when selecting equipment, but they often overlook another critical issue: just because a material can withstand low temperatures doesn’t mean it will maintain adequate impact resistance under those conditions.

Today, starting with material properties and testing methods, we will examine the low-temperature impact risks of casters.

01|Why does low temperature affect the impact resistance of casters?

Common caster wheel materials include polyurethane, rubber, and nylon.

The mechanical properties of these materials may change with temperature.

After the temperature decreases, the molecular chains in some materials lose mobility, resulting in increased rigidity, reduced elasticity, or diminished impact toughness.

When casters pass over floor joints, thresholds, or other localized obstacles, the wheel surface experiences instantaneous forces.

If the material cannot effectively withstand impact at low temperatures, cracks, chipping, or even localized fractures may occur.

It should be noted that the low-temperature performance varies significantly among different material formulations, and one cannot simply assume that a particular material is inherently more resistant to low temperatures.

02 | Are low-temperature resistance and resistance to low-temperature shock the same thing?

The two are related, but not identical.

Low-temperature resistance typically refers to a material’s or product’s ability to maintain its required physical properties and functional performance under specified low-temperature conditions.

Low-temperature impact performance focuses more on a material’s or product’s ability to resist damage when subjected to an instantaneous impact at low temperatures.

For example, after a caster has been left stationary in a low-temperature environment, its wheel body shows no obvious changes in appearance, and rotation remains essentially normal.

However, when the equipment moves and passes over local protrusions, the wheel surface may experience significant instantaneous impacts.

Therefore, a low-temperature standing test alone is insufficient to adequately demonstrate that casters possess good impact resistance during actual movement.

03 | What should be focused on in low-temperature impact testing?

The low-temperature impact verification of casters should be conducted according to a plan developed in consideration of the product’s structure and actual application requirements.

Typically, the following aspects require particular attention.

① Test temperature

The test temperature shall be determined based on the product’s intended service environment.

For applications such as cold storage and cold-chain equipment, the lowest temperature the equipment may actually encounter should be considered, rather than arbitrarily selecting a low-temperature value.

② Low-temperature adjustment time

Prior to testing, the sample must undergo sufficient thermal equilibration under the specified temperature conditions.

If the sample has not yet reached the desired temperature internally, the test results may not accurately reflect the actual low-temperature conditions.

③ Impact Conditions

Different testing objectives may call for different impact methods.

Material-level testing can evaluate the impact performance of specimens; full-wheel testing, on the other hand, can simulate the impacts experienced by a wheel under specified conditions, in accordance with actual service requirements.

The two types of tests cannot be directly equated.

④ Status after testing

After testing is completed, the wheel tread shall be inspected for abnormalities such as cracks, chipping, or fractures, in accordance with the pre-agreed acceptance criteria.

If necessary, further checks should also be carried out to verify the structural integrity of the wheel body and its rolling functionality.

The key to testing is not just whether a crack is present; it is also essential to determine whether the test conditions are relevant to actual operating conditions.

04 | When purchasing casters for cold storage rooms, what issues are easily overlooked?

When purchasing casters for low-temperature environments, you shouldn’t just ask the supplier, “What’s the lowest temperature they can withstand?”

More importantly, it is essential to clarify the following information:

Is there supporting validation data for the product’s applicable temperature range?

How is the impact performance of the wheel tread material at the target low temperature?

Does the equipment need to frequently pass over thresholds, seams, or other obstacles?

Will the casters operate continuously in a low-temperature environment, or will they frequently move between different temperature zones?

Is it necessary to conduct a full-cycle low-temperature operation or impact verification?

In particular, for handling equipment that frequently enters and exits cold storage, the impact of practical factors such as temperature cycling and condensation on product performance should also be considered.

For critical equipment, it is recommended to specify operating conditions and the necessary acceptance criteria in the procurement technical agreement.

05 | The low-temperature casters have developed cracks—can they still be used?

If obvious cracks, chipped edges, or other structural damage are detected on the wheel surface, discontinue abnormal use immediately and inspect or replace the component in accordance with equipment maintenance requirements.

It is not advisable to assume that a wheel can continue to be used normally simply because it is still turning.

At the same time, not all low-temperature cracking issues can be attributed to material quality.

In practice, determining the likely cause of failure also requires considering the impact location, loading conditions, operating temperature, and wheel structure.

Conclusion | When selecting equipment for low-temperature applications, don’t rely solely on temperature ratings.

For cold-chain logistics and low-temperature warehousing equipment, the reliability of casters is not only reflected in their ability to withstand low temperatures, but more importantly, in their ability to meet practical mobility requirements under such conditions.

Casters truly suitable for low-temperature operating conditions must take into account material properties, structural design, impact loads, and the service environment.

GLOBE Universal Casters | Focusing on industrial mobility details to ensure more reliable equipment operation.